Pressure forming

From FabLab Wiki
Jump to navigation Jump to search
Todo for staff
This text needs to be checked

At FabLab Enschede, you can use the Mayku Multiplier to form heated thermoplastic sheets over three-dimensional moulds. Pressure forming is suitable for producing packaging, product housings, prototypes, masks, trays, moulds, and copies of existing shapes.

The Mayku Multiplier is easy to operate yourself after reading this documentation and following the instructions provided at FabLab. You can prepare a mould using your preferred design software, such as SolidWorks, Fusion, FreeCAD, or Blender, or use a suitable existing object.

When you come to FabLab, you can prepare your design using the software on one of our desktop computers. By using our tutorials and FabLab Wiki, we are confident that you will be able to prepare and produce your design yourself. Of course, do not hesitate to ask one of our student assistants for help.

Mayku Multiplier pressure former

About pressure forming

Pressure forming uses heat and compressed air to shape a thermoplastic sheet over a three-dimensional mould. The plastic sheet is heated until it becomes soft. Air pressure then pushes the sheet around the mould, reproducing its shape.

Pressure forming is similar to vacuum forming, but it uses positive air pressure to press the heated sheet over the mould. The Mayku Multiplier can apply a maximum chamber pressure of 60 PSI.

The machine has a standard forming area of 380 × 380 mm and can accommodate moulds up to 160 mm high. A reducing plate is available for smaller products. The reducing plate decreases the usable forming area to approximately 250 × 180 mm, which is roughly A4 size.

The Mayku Multiplier includes default profiles for commonly used materials, including PETG, HIPS, and EVA. These profiles provide suitable starting settings for the full-size forming area.

Important
The quality of a pressure-formed product depends on the mould geometry, mould material, sheet material, sheet thickness, temperature, pressure, heating time, and cooling time. Settings may need to be adjusted after a test forming.

Design a mould

A pressure-forming mould is a three-dimensional object over which the heated plastic sheet is formed. The mould may be designed digitally and manufactured using a 3D printer, CNC milling machine, laser cutter, or another suitable process. A suitable existing object may also be used if it can withstand the temperature and pressure of the forming process.

Software that can be used to design a mould includes: SolidWorks - Fusion - FreeCAD - Blender - Tinkercad

Websites with downloadable three-dimensional models include: Thingiverse - Printables - MakerWorld - MyMiniFactory

Mould design guidelines

A well-designed mould makes it easier to remove the formed plastic without damaging the product or mould.

  • Make sure the mould fits completely within the usable forming area.
  • Include a draft angle on vertical surfaces. Slightly sloped sides make it easier to remove the mould from the formed plastic.
  • Avoid undercuts that mechanically lock the mould inside the formed sheet.
  • Round sharp external corners where possible. Very sharp corners may cause excessive thinning or tearing.
  • Avoid deep, narrow cavities that may be difficult to form.
  • Make sure the mould has a stable and flat base.
  • Keep sufficient space between multiple moulds placed on the forming bed.
  • Make small holes in enclosed or recessed areas when air could otherwise become trapped. These vent holes should connect to the underside of the mould.
  • Make the mould strong enough to resist the selected forming pressure.
  • Use a mould material that can withstand the forming temperature without softening, deforming, or releasing harmful substances.
  • Seal porous mould materials where appropriate.
  • Make sure the mould surface is clean and free from loose particles.
  • Consider how the formed product will be trimmed after forming.
Tip
A mould that is wider at the bottom than at the top may become trapped inside the formed sheet. Add draft angles and avoid undercuts wherever possible.
Warning
Do not use an object as a mould when its material or construction is unknown. Hollow, sealed, fragile, heat-sensitive, pressurised, or electrically powered objects must not be placed in the machine.

Make a pressure-formed product

The basic workflow for making a pressure-formed product is:

  1. Choose the forming area: Decide whether to use the full forming area or the reducing plate.
  2. Prepare the mould: Design and manufacture a suitable mould, or select an existing object that is safe to use.
  3. Inspect the mould: Check the dimensions, draft angles, stability, surface quality, and heat resistance.
  4. Choose the sheet material: Select an approved thermoplastic sheet with a suitable thickness.
  5. Select a profile: Use a default material profile or enter the appropriate settings for the material and forming area.
  6. Install the reducing plate: Install the reducing plate before loading the mould if the smaller forming area is required.
  7. Position the mould: Place the mould securely within the forming area.
  8. Load the sheet: Clamp the thermoplastic sheet into the machine according to the operating instructions.
  9. Check the machine: Confirm the material, sheet thickness, temperature, pressure, heating time, cooling time, and other profile settings.
  10. Start the forming process: Start the cycle and remain near the machine while it heats and forms the sheet.
  11. Allow the product to cool: Do not remove the formed sheet until the cooling cycle has finished and the material is sufficiently rigid.
  12. Remove the forming: Release the frame and carefully remove the sheet and mould.
  13. Separate the mould: Carefully remove the mould without using excessive force.
  14. Trim the product: Cut away excess sheet material using suitable tools.
  15. Inspect the result: Check for insufficient detail, webbing, tearing, excessive thinning, trapped air, or deformation of the mould.
Important
Always perform a test forming when using a new material, a new sheet thickness, a new mould, or an unfamiliar combination of settings.

Available materials

The Mayku Multiplier can form approved thermoplastic sheet materials. Common materials include:

Material Typical applications Notes
PETG Transparent packaging, prototypes, covers, and product housings Commonly used for transparent forming. A default machine profile is available.
HIPS Packaging, prototypes, panels, trays, and model-making Easy to form and trim. A default machine profile is available.
EVA Flexible products, padding, inserts, and soft moulds Flexible material. A default machine profile is available.
ABS Durable housings, prototypes, and functional parts Requires suitable settings and sufficient cooling before removal.
PMMA Transparent covers, displays, and rigid formed parts More rigid than PETG. Forming parameters must be selected carefully.

Material availability may vary. Ask a student assistant when you need a specific material, colour, surface finish, or thickness.

Warning
Only use sheet materials approved by FabLab Enschede. Do not use PVC, unknown plastics, or materials that may release hazardous or corrosive fumes when heated. User-supplied material must be approved before use.

Reducing plate settings

The Mayku Multiplier reducing plate reduces the forming area to approximately 250 × 180 mm.

The following values are starting settings for use with the reducing plate. Actual settings may need to be adjusted for the mould geometry, sheet material, sheet thickness, and required surface detail.

Material Temperature Pressure Forming time Cooling time Heater power Heater-on pressure
1 mm HIPS 160 °C 45 PSI 240 s 120 s 100% 32 PSI
1 mm PETG 160 °C 45 PSI 240 s 120 s 100% 32 PSI
1.5 mm EVA 130 °C 45 PSI 120 s 120 s 100% 28 PSI
4 mm ABS 170 °C 50 PSI 300 s 120 s 60% 10 PSI
3 mm PMMA 165 °C 60 PSI 240 s Not provided Not provided Not provided
Important
The PMMA profile in the available documentation is incomplete. Ask a FabLab employee or student assistant for the missing cooling time, heater power, and heater-on pressure before using this profile.
Tip
Change only one parameter at a time when refining a profile. Record the material, thickness, mould, settings, and result so that successful settings can be reproduced.

Specifications

The table below gives the key specifications of the Mayku Multiplier.

Property Mayku Multiplier
Forming technology Pressure forming
Standard forming area 380 × 380 mm
Maximum mould height 160 mm
Approximate forming area with reducing plate 250 × 180 mm
Maximum chamber pressure 60 PSI
Built-in material profiles PETG, HIPS, EVA, and other supported materials
Important
The mould and plastic sheet must remain within the usable forming area. Allow additional space around the mould so that the sheet can stretch and form correctly.

Safety

The Mayku Multiplier combines high temperatures, compressed air, heated plastic, and moving components. Always follow the FabLab instructions and the operating procedure for the machine.

Warning
The heater, plastic sheet, frame, mould, and formed product can remain hot after the forming cycle. Avoid touching hot surfaces and allow sufficient cooling time.

Before starting

  • Ask a student assistant if you are unsure about the material, mould, or machine settings.
  • Use only materials approved by FabLab Enschede.
  • Make sure the exact material type and sheet thickness are known.
  • Inspect the sheet for contamination, damage, or protective film that must be removed.
  • Check that the mould is heat-resistant, stable, clean, and suitable for pressure forming.
  • Do not use sealed or pressurised objects as moulds.
  • Do not use fragile objects that may collapse or break under pressure.
  • Make sure the mould and sheet fit within the selected forming area.
  • Check that the reducing plate, if used, is installed correctly.
  • Keep the area around the machine clear.

During forming

  • Remain near the machine throughout the forming cycle.
  • Do not touch the heater, heated sheet, forming area, or mould.
  • Keep hands, clothing, hair, tools, and loose objects away from moving and heated parts.
  • Do not try to reposition the mould or sheet after the cycle has started.
  • Do not bypass covers, locks, pressure controls, or other safety features.
  • Stop the machine if you notice unusual sounds, excessive fumes, material burning, uncontrolled deformation, pressure loss, or unexpected movement.
  • Follow the instructed emergency-stop procedure when an unsafe condition occurs.

After forming

  • Wait until the cooling cycle has finished.
  • Check that the material is sufficiently cool and rigid before handling it.
  • Be aware that the mould and inner surfaces may remain hot after the sheet appears cool.
  • Remove the sheet and mould carefully.
  • Use appropriate tools when trimming the formed product.
  • Watch for sharp edges on cut thermoplastic sheets.
  • Clean the machine and surrounding workspace after use.
  • Report damage, unusual machine behaviour, or unsafe conditions to a FabLab employee or student assistant.

Personal protective equipment

Depending on the material and finishing operation, the following personal protective equipment may be required:

  • heat-resistant gloves when handling warm moulds or formed sheets;
  • safety glasses when trimming, drilling, sawing, or otherwise finishing a formed product;
  • suitable cut-resistant gloves when handling sharp sheet edges, provided that these gloves are appropriate for the tool being used;
  • any additional protective equipment specified by FabLab staff.
Important
Gloves must not be worn near rotating cutting tools when they could become caught in the tool. Follow the safety instructions for the selected finishing process.

Tips and tricks

Prevent webbing

Webbing occurs when the sheet folds onto itself between high or closely spaced parts of the mould.

To reduce webbing:

  • increase the spacing between separate moulds;
  • avoid placing tall moulds too close together;
  • use gradual transitions instead of abrupt changes in height;
  • reduce unnecessarily deep features;
  • reposition the moulds on the forming bed;
  • review whether the temperature and heating time are suitable for the sheet.

Improve surface detail

If the formed sheet does not reproduce enough surface detail:

  • check that the sheet has reached the correct forming temperature;
  • make sure the mould contains suitable vent holes;
  • check that recessed areas are not trapping air;
  • verify that the selected pressure is suitable for the material;
  • make sure the mould surface is clean;
  • use a suitable sheet thickness for the required detail.

Make the mould easier to remove

If the mould is difficult to release:

  • increase the draft angle;
  • remove undercuts;
  • round sharp transitions;
  • check whether the plastic has wrapped around the base of the mould;
  • allow the material to cool sufficiently before attempting removal;
  • consider dividing a complex mould into multiple parts.
Warning
Do not use excessive force or sharp metal tools to release a trapped mould. This may damage the product, mould, or machine and can cause injury. Ask a student assistant for help.

Keep a record of successful profiles

For repeatable results, record:

  • material type;
  • sheet thickness;
  • sheet manufacturer or supplier;
  • mould material;
  • mould dimensions;
  • forming area or reducing plate;
  • temperature;
  • pressure;
  • heating and forming time;
  • cooling time;
  • heater power;
  • heater-on pressure;
  • observed result and any defects.

Troubleshooting

Problem Possible cause Recommended action
The sheet does not reproduce enough detail The sheet is not sufficiently heated, the pressure is too low, or air is trapped around the mould Check the material profile, mould vents, forming temperature, and pressure. Ask a student assistant before increasing settings.
The sheet tears The sheet is too hot, stretched too far, or too thin for the mould geometry Reduce severe height changes, round sharp corners, check the heating settings, or select a more suitable sheet thickness.
Webbing forms between parts Moulds are too close together or the geometry causes the sheet to fold Increase spacing, reposition the moulds, or simplify the mould geometry.
The mould is trapped The mould contains insufficient draft or an undercut Allow the sheet to cool and ask a student assistant for help. Redesign the mould before repeating the job.
The mould deforms The mould material is not sufficiently heat-resistant or strong Stop using the mould and replace it with a suitable mould made from an approved material.
The formed product is distorted after removal The product was removed before it had cooled sufficiently Increase the cooling time and allow the product to become rigid before removing it.
Bubbles or surface defects appear The sheet may contain moisture, contamination, or unsuitable protective film Check the sheet preparation and material instructions. Use clean, approved material.
Excessive fumes or an unusual smell occurs The material may be unsuitable, contaminated, or overheated Stop the cycle, keep clear of the machine, and contact a FabLab employee or student assistant.
Warning
Stop the machine and ask a FabLab employee or student assistant for help if the recommended troubleshooting steps do not resolve the problem. Do not continue operating the machine when the material, mould, pressure system, or heater behaves unexpectedly.